AMS2759/2K Heat Treatment of Low-Alloy Steel Parts Minimum Tensile Strength 220 ksi (1517 MPa) and Higher

Revised

07/07/2021

Features
Issuing Committee
Scope
Content
This specification, in conjunction with the general requirements for steel heat treatment covered in AMS2759, establishes the requirements for heat treatment of low-alloy steel parts to minimum ultimate tensile strengths of 220 ksi (1517 MPa) and higher. Parts are defined in AMS2759. The requirements for heat treatment of alloy Aermet100 are no longer part of this specification and can be found in AMS2759/3. Due to the limited hardenability of these materials, size limits have been added to this specification.
Meta TagsDetails
DOI
https://doi.org/10.4271/AMS2759/2K
Pages
15
Citation
SAE International Material Specification, Heat Treatment of Low-Alloy Steel Parts Minimum Tensile Strength 220 ksi (1517 MPa) and Higher, SAE Standard AMS2759/2K, Revised July 2021, Reaffirmed April 2014, Issued October 1984, https://doi.org/10.4271/AMS2759/2K.
Additional Details
Publisher
Published
Jul 7, 2021
Product Code
AMS2759/2K
Content Type
Material Specification
Status
Revised
Language
English