This specification, in conjunction with the general requirements for steel heat treatment covered in AMS 2759, establishes the requirements for heat treatment of low-alloy steel parts to minimum ultimate tensile strengths of 220 ksi (1517 MPa) and higher. Parts are defined in AMS 2759.
Rationale
Content
AMS 2759/2D results from a Five Year Review and update to include in Table 2 Note 5 clarification that the snap temper is employed before refrigeration. AMS 2759/2D also includes use of marquenching.
Meta TagsDetails
DOI
https://doi.org/10.4271/AMS2759/2D
Pages
12
Citation
SAE International Material Specification, Heat Treatment of Low-Alloy Steel Parts Minimum Tensile Strength 220 ksi (1517 MPa) and Higher, SAE Standard AMS2759/2D, Revised August 2007, Issued October 1984, https://doi.org/10.4271/AMS2759/2D.
Additional Details
Publisher
Published
Aug 24, 2007
Product Code
AMS2759/2D
Content Type
Material Specification
Status
Revised
Language
English