AMS2759/2C Heat Treatment of Low-Alloy Steel Parts Minimum Tensile Strength 220 ksi (1517 MPa) and Higher
Revised
09/01/2000
- Features
- Issuing Committee
- Content
- This specification, in conjunction with the general requirements for steel heat treatment covered in AMS 2759, establishes the requirements for heat treatment of low-alloy steel parts to minimum ultimate tensile strengths of 220 ksi (1517 MPa) and higher. Parts are defined in AMS 2759.
- Pages
- 13
- Citation
- SAE International Material Specification, Heat Treatment of Low-Alloy Steel Parts Minimum Tensile Strength 220 ksi (1517 MPa) and Higher, SAE Standard AMS2759/2C, Revised September 2000, Issued October 1984, https://doi.org/10.4271/AMS2759/2C.