AMS2759/2B HEAT TREATMENT OF LOW-ALLOY STEEL PARTS Minimum Tensile Strength 220 ksi (1517 MPa) and Higher
Revised
12/01/1996
- Features
- Issuing Committee
- Content
- This specification, in conjunction with the general requirements for steel heat treatment covered in AMS 2759, establishes the requirements for heat treatment of low-alloy steel parts to minimum ultimate tensile strengths of 220 ksi (1517 MPa) and higher. Parts are defined in AMS 2759.
- Pages
- 13
- Citation
- SAE International Material Specification, HEAT TREATMENT OF LOW-ALLOY STEEL PARTS Minimum Tensile Strength 220 ksi (1517 MPa) and Higher, SAE Standard AMS2759/2B, Revised December 1996, Issued October 1984, https://doi.org/10.4271/AMS2759/2B.