AMS2759/2 Heat Treatment of Low-Alloy Steel Parts Minimum Tensile Strength 220 ksi (1517 MPa) and Higher

Reaffirmed

08/10/2011

Scope
Content
This specification, in conjunction with the general requirements for steel heat treatment covered in AMS2759, establishes the requirements for heat treatment of low-alloy steel parts to minimum ultimate tensile strengths of 220 ksi (1517 MPa) and higher. Parts are defined in AMS2759.
Meta TagsDetails
DOI
https://doi.org/10.4271/AMS2759/2
Pages
12
Citation
SAE International Material Specification, Heat Treatment of Low-Alloy Steel Parts Minimum Tensile Strength 220 ksi (1517 MPa) and Higher, SAE Standard AMS2759/2, Reaffirmed August 2011, Issued September 1996, https://doi.org/10.4271/AMS2759/2.