AS7482A Studs, Corrosion and Heat Resistant Steel, UNS S66286 Tensile Strength 130 ksi 1800 °F Solution Heat Treated, Aged Before Roll Threading Procurement Specification
Reaffirmed
05/08/2006
- Features
- Issuing Committee
- Content
- This specification covers studs made from a corrosion and heat resistant, age hardenable iron base alloy of the type identified under the Unified Numbering System as UNS S66286. The following specification designations and their properties are covered:
- Pages
- 21
- Citation
- SAE International Technical Standard, Studs, Corrosion and Heat Resistant Steel, UNS S66286 Tensile Strength 130 ksi 1800 °F Solution Heat Treated, Aged Before Roll Threading Procurement Specification, SAE Standard AS7482A, Reaffirmed May 2006, Revised October 1996, Issued October 1991, https://doi.org/10.4271/AS7482A.