AS7482 STUDS, STEEL, CORROSION AND HEAT RESISTANT 1800°F Solution Heat Treated Precipitation Heat Treated Before Roll Threaded

Reaffirmed

08/16/2011

Features
Issuing Committee
Scope
Content
This procurement specification covers aircraft quality studs made from a corrosion and heat resistant age hardenable iron base alloy of the type identified under the Unified Numbering System as UNS S66286 and of 130 000 psi tensile strength at room temperature, with maximum test temperature of parts at 1200°F.
Meta TagsDetails
DOI
https://doi.org/10.4271/AS7482
Pages
21
Citation
SAE International Technical Standard, STUDS, STEEL, CORROSION AND HEAT RESISTANT 1800°F Solution Heat Treated Precipitation Heat Treated Before Roll Threaded, SAE Standard AS7482, Reaffirmed May 1995, Issued January 1991, https://doi.org/10.4271/AS7482.
Additional Details
Publisher
Published
Aug 16, 2011
Product Code
AS7482
Content Type
Technical Standard
Status
Reaffirmed
Language
English

Revisions