ARP1631A Manufacturing Sequence for Fabrication of High-Strength Steel Parts 300M or 4340 Modified Low-Alloy Steels 270,000 psi (1860 MPa) Tensile Strength and Higher
Reaffirmed
06/24/2024
- Features
- Issuing Committee
- Content
- This document establishes the requirements for the sequencing of processes relating to parts fabricated from 300M or 4340 modified steel heat treated to, or to be heat treated to, 270,000 psi (1860 MPa) minimum ultimate tensile strength (UTS) and higher.
- Pages
- 12
- Citation
- SAE International Recommended Practice, Manufacturing Sequence for Fabrication of High-Strength Steel Parts 300M or 4340 Modified Low-Alloy Steels 270,000 psi (1860 MPa) Tensile Strength and Higher, SAE Standard ARP1631A, Reaffirmed June 2024, Revised November 2007, Issued October 1984, https://doi.org/10.4271/ARP1631A.