ARP1631 MANUFACTURING SEQUENCE FOR FABRICATION OF HIGH-STRENGTH STEEL PARTS 300M or 4340 Modified Low-Alloy Steels 270,000 psi (1860 MPa) Tensile Strength and Higher

Current

10/01/1984

Features
Issuing Committee
Scope
Content
This document establishes the requirements for the sequencing of processes relating to parts fabricated from 300M or 4340 modified steel heat treated to, or to be heat treated to, 270,000 psi (1,860 MPa) minimum ultimate tensile strength (UTS) and higher.