J467_196810 Special Purpose Alloys ("Superalloys")

Revised

10/1/1968

Scope
Content
<![CDATA[ABSTRACT]]> The data given in Tables 1-4 are typical values only and are not intended for design parameters. Mechanical properties of the special purpose alloys depend greatly upon processing variables and heat treatment. It is recommended that design data be obtained by actual testing or by consultation with the producers of the alloys.
Meta Tags
Topics
Details
DOI
https://doi.org/10.4271/J467_196810
Citation
SAE International Technical Standard, Special Purpose Alloys ("Superalloys"), SAE Standard J467_196810, Revised October 1968, Revised October 1968, https://doi.org/10.4271/J467_196810.