ARP982C Minimizing Stress-Corrosion Cracking in Wrought Titanium Alloy Products
Reaffirmed
12/19/2002
- Content
- Primarily to provide recommendations concerning minimizing stress-corrosion cracking in wrought titanium alloy products.
- Citation
- SAE International Recommended Practice, Minimizing Stress-Corrosion Cracking in Wrought Titanium Alloy Products, SAE Standard ARP982C, Reaffirmed December 2002, Revised March 1997, Issued November 1967, https://doi.org/10.4271/ARP982C.