ARP1110D Minimizing Stress Corrosion Cracking in Wrought Forms of Steels and Corrosion Resistant Steels and Alloys
Revised
1/21/2021
- Content
- The purpose of this SAE Aerospace Recommended Practice (ARP) is to provide the aerospace industry with recommendations concerning the minimization of stress corrosion cracking in wrought heat-treatable carbon and low alloy steels and in austenitic, precipitation hardenable, and martensitic corrosion-resistant steels and alloys.The detailed recommendations are based on laboratory and field experience and reflect those design practices and fabrication procedures which should avoid in-service stress corrosion cracking.
- Citation
- SAE International Recommended Practice, Minimizing Stress Corrosion Cracking in Wrought Forms of Steels and Corrosion Resistant Steels and Alloys, SAE Standard ARP1110D, Revised March 2026, Reaffirmed April 2011, https://doi.org/10.4271/ARP1110D.