Content
This specification covers a high strength, corrosion and heat-resistant cobalt-nickel-chromium alloy in the form of bars.
Meta TagsDetails
DOI
https://doi.org/10.4271/AMS5843E
Pages
5
Citation
SAE International Material Specification, Cobalt-Nickel Alloy, Corrosion and Heat-Resistant, Bars 19Cr - 36Co - 25Ni - 7.0Mo - 0.50Cb (Nb) - 2.9Ti - 0.20Al - 9.0Fe Vacuum Induction Plus Vacuum Consumable Electrode Melted Solution Heat Treated, Work Strengthened, and Aged, SAE Standard AMS5843E, Revised August 2006, Issued March 1977, https://doi.org/10.4271/AMS5843E.
Additional Details
Publisher
Published
Aug 3, 2006
Product Code
AMS5843E
Content Type
Material Specification
Status
Revised
Language
English