AMS5841D Cobalt-Nickel Alloy, Corrosion and Heat Resistant, Bars 19Cr - 36Co - 25Ni - 7.0Mo - 0.50Cb - 2.9Ti - 0.20Al - 9.0Fe Vacuum Induction Plus Vacuum Consumable Electrode Melted Solution Heat Treated for Work Strengthening
Revised
10/01/2000
- Features
- Issuing Committee
- Content
- This specification covers a high strength, corrosion and heat resistant cobalt-nickel-chromium alloy in the form of bars.
- Pages
- 7
- Citation
- SAE International Material Specification, Cobalt-Nickel Alloy, Corrosion and Heat Resistant, Bars 19Cr - 36Co - 25Ni - 7.0Mo - 0.50Cb - 2.9Ti - 0.20Al - 9.0Fe Vacuum Induction Plus Vacuum Consumable Electrode Melted Solution Heat Treated for Work Strengthening, SAE Standard AMS5841D, Revised October 2000, Issued March 1977, https://doi.org/10.4271/AMS5841D.