AMS5709K Nickel Alloy, Corrosion- and Heat-Resistant, Bars and Forgings, 58Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al - 0.05Zr - 0.006B, Consumable Electrode or Vacuum Induction Melted, 1975 °F (1079 °C) Solution Heat Treated, Stabilized, and Precipitation Heat Treated
Revised
05/03/2025
- Features
- Issuing Committee
- Content
- This specification covers a corrosion- and heat-resistant nickel alloy in the form of bars and forgings in the solutioned, stabilized, and precipitation heat-treated condition. Stock for forging shall be in the condition ordered.
- Pages
- 7
- Citation
- SAE International Material Specification, Nickel Alloy, Corrosion- and Heat-Resistant, Bars and Forgings, 58Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al - 0.05Zr - 0.006B, Consumable Electrode or Vacuum Induction Melted, 1975 °F (1079 °C) Solution Heat Treated, Stabilized, and Precipitation Heat Treated, SAE Standard AMS5709K, Revised May 2025, Reaffirmed December 2013, Issued July 1963, https://doi.org/10.4271/AMS5709K.