AMS5637F Steel, Corrosion Resistant, Bars and Wire 18Cr - 9.0Ni (SAE 30302) Solution Heat Treated and Cold Drawn 125 ksi (862 MPa) Tensile Strength
Reaffirmed
08/01/2000
- Features
- Issuing Committee
- Content
- This specification covers a corrosion resistant steel in the form of bars and wire 0.75 inch (19 mm) and under in nominal diameter or distance between parallel sides.
- Pages
- 6
- Citation
- SAE International Material Specification, Steel, Corrosion Resistant, Bars and Wire 18Cr - 9.0Ni (SAE 30302) Solution Heat Treated and Cold Drawn 125 ksi (862 MPa) Tensile Strength, SAE Standard AMS5637F, Reaffirmed August 2000, Revised October 1993, Issued March 1949, https://doi.org/10.4271/AMS5637F.