AMS5590C NICKEL ALLOY, CORROSION AND HEAT RESISTANT, SEAMLESS TUBING 52.5Ni - 19Cr - 3.0Mo - 5.1(Cb + Ta) - 0.90Ti - 0.50Al - 18Fe Consumable Electrode or Vacuum Induction Melted 1950 °F (1066 °C) Solution Heat Treated
Revised
04/01/1993
- Features
- Issuing Committee
- Content
- This specification covers a corrosion and heat resistant nickel alloy in the form of seamless tubing.
- Pages
- 8
- Citation
- SAE International Material Specification, NICKEL ALLOY, CORROSION AND HEAT RESISTANT, SEAMLESS TUBING 52.5Ni - 19Cr - 3.0Mo - 5.1(Cb + Ta) - 0.90Ti - 0.50Al - 18Fe Consumable Electrode or Vacuum Induction Melted 1950 °F (1066 °C) Solution Heat Treated, SAE Standard AMS5590C, Revised April 1993, Issued September 1966, https://doi.org/10.4271/AMS5590C.