This specification covers a corrosion and heat-resistant nickel alloy in the form of seamless tubing 0.125 inch (3.18 mm) and over in nominal OD with nominal wall thickness 0.015 inch (0.38 mm) and over (see 8.6).
Rationale
Content
AMS5589G prohibits unauthorized exceptions (3.9), revises Composition (3.1) to remove test procedures, Fabrication (3.4), Hardness (3.6.2.2), clarifies stress-rupture testing for small diameter or thin wall tubing (3.6.2.3.3), revises Quality (3.7.1), Reports (4.4.1) and Identification (5.2.1), and results from a Five-Year Review and update of this specification.
Meta TagsDetails
DOI
https://doi.org/10.4271/AMS5589G
Pages
7
Citation
SAE International Material Specification, Nickel Alloy, Corrosion and Heat-Resistant, Seamless Tubing 52.5Ni - 19Cr - 3.0Mo - 5.1Cb (Nb) 0.90Ti - 0.50Al - 18Fe Consumable Electrode Remelted or Vacuum Induction Melted 1775 °F (968 °C) Solution Heat Treated, SAE Standard AMS5589G, Revised December 2019, Issued September 1996, https://doi.org/10.4271/AMS5589G.
Additional Details
Publisher
Published
Dec 13, 2019
Product Code
AMS5589G
Content Type
Material Specification
Status
Revised
Language
English