This specification covers a corrosion- and heat-resistant nickel alloy in the form of bars, forgings, and flash welded rings in the solution heat-treated condition, 5 inches (127 mm) and under in nominal diameter or least distance between parallel sides (thickness) having a maximum cross-sectional area of 50 square inches (323 cm2), and stock of any size for forging, flash welded rings, or heading.
Rationale
Content
AMS5441C is the result of a Five-Year Review and update of the specification. The revision clarifies the condition and size limits (1.1), updates composition testing and reporting (3.1, 3.1.1), updates Table 2 test methods, limits hardness test options (3.5.1.1.1, 3.5.1.2.2), adds pyrometry control (3.5.1.2), adds strain control (3.5.1.2.1.5), allows prior revisions (8.4), and prohibits unauthorized exceptions (3.8, 4.4.2, 4.4.3, 5.2.1.1, 8.5).
Meta TagsDetails
DOI
https://doi.org/10.4271/AMS5441C
Pages
9
Citation
SAE International Material Specification, Nickel Alloy, Corrosion- and Heat-Resistant, Bars, Forgings, and Rings Ni - 18Cr - 2.8Mo - 5.5Cb (Nb) - 0.70Ti - 1.50Al - 10Fe - 9Co - 1W Consumable Electrode Remelted or Vacuum Induction Melted 1775 °F (968 °C) Solution Heat Treated, Precipitation-Hardenable, SAE Standard AMS5441C, Revised April 2023, Issued September 2006, https://doi.org/10.4271/AMS5441C.
Additional Details
Publisher
Published
Apr 4, 2023
Product Code
AMS5441C
Content Type
Material Specification
Status
Revised
Language
English

Revisions