AMS5410B Nickel Alloy, Corrosion and Heat Resistant, Investment Castings 61Ni - 16Cr - 8.5Co - 1.8Mo - 2.6W - 0.85Cb - 3.4Ti - 1.8Ta - 3.4Al - 0.010B - 0.05Zr Vacuum Melted, Vacuum Cast As Cast, or Solution Treated, or Solution and Precipitation Hardened
Revised
07/13/2010
- Features
- Issuing Committee
- Content
- This specification covers a corrosion and heat resistant vacuum melted nickel alloy in the form of investment castings.
- Pages
- 11
- Citation
- SAE International Material Specification, Nickel Alloy, Corrosion and Heat Resistant, Investment Castings 61Ni - 16Cr - 8.5Co - 1.8Mo - 2.6W - 0.85Cb - 3.4Ti - 1.8Ta - 3.4Al - 0.010B - 0.05Zr Vacuum Melted, Vacuum Cast As Cast, or Solution Treated, or Solution and Precipitation Hardened, SAE Standard AMS5410B, Revised July 2010, Reaffirmed April 2006, Issued October 1984, https://doi.org/10.4271/AMS5410B.