AMS5342A STEEL CASTINGS, INVESTMENT, CORROSION RESISTANT 16Cr - 4.1Ni - 0.28 (Cb+Ta) - 3.2Cu Solution and Precipitation Heat Treated 130,000 psi (896 MPa) Tensile Strength

Revised

07/01/1977

Features
Issuing Committee
Scope
Content
This specification covers a corrosion-resistant steel in the form of investment castings.