- This specification, in conjunction with the general requirements for steel heat treatment covered in AMS2759, establishes the requirements for heat treatment of carbon and low-alloy steel parts to minimum ultimate tensile strengths below 220 ksi (1517 MPa). Parts are defined in AMS2759. Due to limited hardenability in these materials, there are size limits in this specification.
- Pages
- 16
- Citation
- SAE International Material Specification, Heat Treatment of Carbon and Low-Alloy Steel Parts Minimum Tensile Strength Below 220 ksi (1517 MPa), SAE Standard AMS2759/1G, Revised June 2019, Reaffirmed April 2014, Issued October 1984, https://doi.org/10.4271/AMS2759/1G.