Study of the Microstructural Behavior of the Ti-6Al-4V Alloy in Creep Test at 600°C

2007-01-2807

11/28/2007

Authors
Abstract
Content
The objective of this work was evaluating the microstructure of the Ti-6Al-4V alloy in creep test. Yttria stabilized zirconia with a CoNiCrAlY bond coat was atmospherically plasma sprayed on substrate. Constant load creep tests were conducted with alloy in air and in nitrogen atmospheres at stress level of 319 MPa at 600°C. The microstructural analyze shows that the predominant mechanism in the test conditions was characterized by formation and coalescence of microcavities with shape and size varieties. The size and shape of dimples are governed by number and distribution of nucleated microcavities and by stress internal level present in material.
Meta TagsDetails
DOI
https://doi.org/10.4271/2007-01-2807
Citation
Reis, D., da Silva Briguente, L., Cortez, L., Neto, F., et al., "Study of the Microstructural Behavior of the Ti-6Al-4V Alloy in Creep Test at 600°C," SAE Brasil 2007 Congress and Exhibit, Sao Paulo, Brazil, November 28, 2007, https://doi.org/10.4271/2007-01-2807.
Additional Details
Publisher
Published
11/28/2007
Product Code
2007-01-2807
Content Type
Technical Paper
Language
English