Study of the Fractography of Inconel 718 Superalloy After Creep Mechanical Test

2011-36-0401

10/4/2011

Authors
Abstract
Content
This work intends to analyze the influence of the stress and temperatures used in creep mechanical tests in the types of fractures that occurred in the superalloy Inconel 718. For this, the superalloy was subjected to creep tests under the conditions 625 to 814 MPa at temperatures of 650, 675 and 700°C. After the tests, the fractured samples were cleaned on an ultrasound and subjected to microstructural analysis using the technique of scanning electron microscopy. Images were performed with different increases in order to analyze the type of fracture that occurred in the material. The elongated sample and its reduction in area were also measured in order to study the effects of different conditions used in the creep tests under material's fracture.
Meta TagsDetails
DOI
https://doi.org/10.4271/2011-36-0401
Citation
Sugahara, T., Reis, D., de Moura Neto, C., and Piorino Neto, F., "Study of the Fractography of Inconel 718 Superalloy After Creep Mechanical Test," SAE Brasil 2011 Congress and Exhibit, Sao Paulo, Brazil, October 4, 2011, https://doi.org/10.4271/2011-36-0401.
Additional Details
Publisher
Published
10/4/2011
Product Code
2011-36-0401
Content Type
Technical Paper
Language
English