Novel Low Profiling RIM Resin for Exterior Body Panel Applications
870280
02/23/1987
- Event
- Content
- The production of FRP Class A surface parts for the automotive industry has been limited to high temperature SMC molding which requires chrome plated steel tooling and large hydraulic presses. The cost of this type of operation limits the economics of the process to a minimum of 30,000 parts/yr. Production runs of 3,000 to 20,000 parts/yr cannot justify hard tooling so other methods of production are used. These alternate methods have not offered the same quality of surface as the high temperature molding does.A new resin transfer molding resin. Arotran™ 50437, has been developed which can be used at mold temperatures as low as 120°F. Parts have been produced at tool temperatures between 120°F and 200°F with a surface comparable to that obtained with SMC. Molding produced at 120°F have utilized plastic tooling. Processing at 200°F, however, will undoubtedly require more durable tooling such as nickel shell molds.
- Pages
- 6
- Citation
- Jensen, J., and Vaccarella, P., "Novel Low Profiling RIM Resin for Exterior Body Panel Applications," SAE Technical Paper 870280, 1987, https://doi.org/10.4271/870280.