Traditional cemented carbides struggle to simultaneously improve hardness and toughness, and cobalt scarcity further limits their industrial production. To address these limitations, we utilize CoCrFeNi (with good ductility) as the binder phase to fabricate CoCrFeNi/WC cemented carbides, and regulate sintering temperature (1100-1200 °C) and holding time (3-10 min) to tailor the microstructure and mechanical properties, focusing on the occurrence of residual binder phase. The results indicate that sintering parameters significantly affect the morphology and content of residual binder phases: elliptical phases form at 1100 °C, while strip-like phases dominate at 1150-1200 °C. Specifically, the MEA3 sample sintered at 1200 °C for 10 min achieves the best mechanical balance (Vickers hardness: 2281 HV; fracture toughness: 12.2 MPa·m^1/2), attributed to reduced residual binder phase fraction and enhanced densification, which improve interfacial bonding. In contrast, a relatively high content of residual binder phases induced by lower temperatures (e.g., 1100 °C) or inappropriate holding times degrades mechanical properties. Microstructure analysis confirms that rational sintering optimization is key to controlling residual binder phase evolution and realizing high-performance cemented carbides. This study provides an experimental basis for the industrial production of high-performance WC-based carbides.
Meta TagsDetails
DOI
https://doi.org/10.4271/2026-99-2308
Citation
Sun, Y., Li, P., and Ma, Z., "Microstructure and Properties of CoCrFeNi/WC Cemented Carbides," 2026 2nd International Conference on Aerospace Engineering and Materials Technology, Xi'An, China, April 10, 2026, https://doi.org/10.4271/2026-99-2308.
Additional Details
Publisher
Published
Oct 30
Product Code
2026-99-2308
Content Type
Technical Paper
Language
English