Galvanic Corrosion of Die Cast Magnesium Exposed on Vehicles and in Accelerated Laboratory Tests
2006-01-0255
04/03/2006
- Event
- Content
- Galvanic corrosion between die cast AZ91D and AM60B and different fastener systems has been evaluated by exposure on trucks and in accelerated laboratory tests. The exposure time on the trucks was 3 years, corresponding to a mileage of about 300000 km. Samples were retracted and evaluated after 1 and 2 years exposure. Similar samples were also exposed to the Volvo Indoor Corrosion Test and the General Motors GM9540P-cycle B test. The correlation between the field data and the laboratory tests was evaluated, as was the sharp difference in the performance of the fastener systems in the two accelerated laboratory tests.