Development of Nickel-Base Superalloy for Exhaust Valves
910429
2/1/1991
- Content
- These days, nickel-base superalloy has been applied to reduce the valve weight of motorcycles. Inconel 751 is excellent in performance but expensive in cost. Therefore, we verified the constituents of nickel-base superalloys corresponding to the requirements of valves and we succeeded in developing a new superalloy and applying it to motorcycle exhaust valves.The characteristics are summarized as follows:
-
1.
The basic composition is Fe-46Ni-18Cr-4Ti-1Al-0.3C-0.004B. It is a precipitation-hardened nickel alloy characterized by precipitation of Ni3 (Al,Ti) and, crystallization and dispersion of fine TiC.
-
2.
It has the following distinctive features.
-
(1)
Superior to Inconel 751 in wear and heat resistance.
-
(2)
Superior to 20-11P steel in resistance to lead oxide corrosion.
-
(3)
Applicable to both unleaded and low-lead gasoline.
-
(1)
-
3.
The exhaust valves using this new superalloy are lighter in weight by 18% and lower in cost by 13% as compared to the conventional type using 20-11P hard-faced with Stellite. They have been mass-produced from 1990.
-
1.
- Citation
- Hagiwara, Y., Ishida, M., Oka, T., Watanabe, R., et al., "Development of Nickel-Base Superalloy for Exhaust Valves," International Congress & Exposition, Detroit, Michigan, United States, February 25, 1991, https://doi.org/10.4271/910429.