Using standard tensile testing methods, the material properties of AKDQ and DP600 steels tubes along the axial direction were determined. A novel in-situ optical strain mapping system ARAMIS® was utilized to evaluate the strain distribution during tensile testing along the axial direction. Microstructural and damage characterization was carried out using microscopy and image analysis techniques to compare the damage evolution and formability of both materials. Failure in both steels was observed to occur via a ductile failure mode. AKDQ was found to be the more formable material as it can achieve higher strains, total elongations and thinning prior to failure than the higher strength DP600.
Meta TagsDetails
DOI
https://doi.org/10.4271/2005-01-0092
Pages
9
Citation
Winkler, S., Bardelcik, A., Worswick, M., Ososkov, Y. et al., "Damage and Formability of AKDQ and High Strength DP600 Steel Tubes," SAE Technical Paper 2005-01-0092, 2005, https://doi.org/10.4271/2005-01-0092.
Additional Details
Publisher
Published
Apr 11, 2005
Product Code
2005-01-0092
Content Type
Technical Paper
Language
English