AMS5843H Cobalt-Nickel Alloy, Corrosion- and Heat-Resistant, Bars 19Cr - 36Co - 25Ni - 7.0Mo - 0.50Cb (Nb) - 2.9Ti - 0.20Al - 9.0Fe Vacuum Induction Plus Vacuum Consumable Electrode Melted Solution Heat Treated, Work Strengthened, and Aged

Revised

09/08/2022

Features
Issuing Committee
Scope
Content
This specification covers a high strength, corrosion- and heat-resistant cobalt-nickel-chromium alloy in the form of bars 1-3/4 inches (44.4 mm) and under in nominal diameter.
Rationale
Content
AMS5843G is the result of a Five-Year Review and update of the specification. The revision prohibits unauthorized exceptions (3.6, 3.9, 4.4.2, 5.2.1, 8.6) and establishes associated size limits (1.1), updates composition testing and reporting (3.1, 3.1.1), prohibits bar cut from plate (3.3.1, 4.4.1), adds strain rate control for tensile tests (3.5.1.3), adds reporting requirement for stress rupture testing (3.5.4.3), and allows prior revisions (8.5).
Meta TagsDetails
DOI
https://doi.org/10.4271/AMS5843H
Pages
7
Citation
SAE International Material Specification, Cobalt-Nickel Alloy, Corrosion- and Heat-Resistant, Bars 19Cr - 36Co - 25Ni - 7.0Mo - 0.50Cb (Nb) - 2.9Ti - 0.20Al - 9.0Fe Vacuum Induction Plus Vacuum Consumable Electrode Melted Solution Heat Treated, Work Strengthened, and Aged, SAE Standard AMS5843H, Revised September 2022, Issued March 1977, https://doi.org/10.4271/AMS5843H.
Additional Details
Publisher
Published
Sep 8, 2022
Product Code
AMS5843H
Content Type
Material Specification
Status
Revised
Language
English