Nickel Alloy, Corrosion and Heat Resistant, Seamless Tubing 52.5Ni - 19Cr - 3.0Mo - 5.1Cb - 0.90Ti - 0.50Al - 18Fe Consumable Electrode or Vacuum Induction Melted 1775 °F (968 °C) Solution Heat Treated
- Aerospace Material Specification
- AMS5589D
- Revised
Scope
Recommended Content
Topic
Data Sets - Support Documents
Title | Description | Download |
---|---|---|
Unnamed Dataset 1 | ||
Unnamed Dataset 2 | ||
TABLE 1 | Composition | |
TABLE 2 | Tensile Properties | |
TABLE 3 | Minimum Tensile Properties | |
TABLE 4A | Large Tubing Tolerances, Inch/Pound Units | |
TABLE 4B | Large Tubing Tolerances, SI Units |
Issuing Committee
AMS F Corrosion and Heat Resistant Alloys Committee
The committee of Corrosion and Heat Resistant Steels and Alloys and Specialty Steels and Alloys, AMS Committee F, will prepare, coordinate, and revise documents related to corrosion and heat resistant steels and alloys and specialty steels and alloys technology, such as stainless steels and nickel and base alloys, through the participation of metals suppliers, users, and interested government agencies. Committee activities shall provide a forum for the cooperative interchange of ideas and experience of the participants, resulting in the publication of specifications that embody sound, established aerospace industry practices and requirements to serve the suppliers and customers of aerospace materials.