Abstract
Content

The protection of cathodic metallic materials used for aircraft components, like 4340, Aermet 100, and PH 13-8 corrosion-resistant steel, is critical to keeping the steel from pitting and cracking due to exposure to the operating environment. Two important properties are resistance to stress-corrosion cracking (SCC) and corrosion fatigue. These are insidious failure mechanisms that can lead to part failure in service.