Several recently formulated nickelbase superalloys have been developed with excellent high-temperature creep resistance, at lower densities than those of currently used nickel-base superalloys. These alloys are the latest products of a continuing effort to develop alloys that have even greater strength-toweight ratios, suitable for use in turbine blades of aircraft engines. Mass densities of turbine blades exert a significant effect on the overall weight of aircraft. For a given aircraft, a reduction in the density of turbine blades enables design reductions in the weight of other parts throughout the turbine rotor, including the disk, hub, and shaft, as well as supporting structures in the engine. The resulting total reduction in weight can be 8 to 10 times that of the reduction in weight of the turbine blades.

Meta TagsDetails
Citation
"Low-Density, Creep Resistant Single Crystal Superalloys," Mobility Engineering, July 1, 2006.
Additional Details
Publisher
Published
7/1/2006
Product Code
TBMG-90
Content Type
Magazine Article
Language
English