Electron-Beam Welding of Superalloys at High Temperatures

TBMG-3059

3/1/2002

Abstract
Content

Electron-beam welding at high temperatures has been found to be a suitable process for joining structural components made by casting certain superalloys. This process can be used in the fabrication of superalloy parts that must withstand high operating temperatures. Examples of such parts include exhaust ducts of advanced aerospace engines and end caps on turbine buckets.