AS6507 Test Method and Limits for Bow Height of Aluminum Sheet Samples After Chemical Milling

Reaffirmed

11/02/2021

Features
Issuing Committee
Scope
Content
The results of this test are intended to be a useful indication of the resistance to distortion of bare or two-side Alclad, flat sheet aluminum used in chemical milling applications.
Rationale
Content
This new SAE Aerospace Standard (AS) defines the test method and limits for the bow height of aluminum sheet samples after chemical milling.