Abstract
Spring steels are the materials most commonly used in suspensions of vehicles and are subject to heavy efforts in terms of load, impact and also under intense fatigue solicitation. Required mechanical performance depends mainly on the chemical composition and heat treatments. Therefore, the aim of the present work was to compare SAE 5160 steel with one Super Clean steel developed in Slovenia. Searches improving mechanical properties of these steels are constantly present in the automotive industry, reducing vehicle weight and maintaining safety. In this scenario, cryogenic treatment in combination with quenching and tempering has shown interesting results in the scientific literature for tool steels and the best results for cryogenics are achieved when the treatment occurs for long duration as 24 hours. However, for the industry, the production lead time should be as fast as possible, then it is interesting to discern the influence on spring steels of cryogenics when shorter durations as 12 hours, 2 hours and 30 minutes. The parameters that measure the ability of these materials to resist the quick fracture are called fracture toughness. Standardized tests are difficult to apply, so an alternative fracture toughness testing developed in IMT (Institute of Metals and Technology), Ljubljana, Slovenia, is one of the most promising methods. Thus, after applying these tests, the Super Clean steel showed higher resistance than SAE 5160 and there was not any enhancement caused by cryogenics.
Authors
Topic
Citation
Gonçalves, V., Canale, L., Leskovšek, V., and Podgornik, B., "Influence of Cryogenic Treatment on the Fracture Toughness of Conventional and Super Clean Spring Steels," SAE Technical Paper 2016-36-0064, 2016, https://doi.org/10.4271/2016-36-0064.Also In
References
- Chiaverini , V. Aços-Carbono e Aços-Liga Publication of Metals Brazilian Association (ABM) 3 São Paulo 1971
- Favorit Technical Catalogue 12 Aços Favorit Distribuidora Ltda Company Cachoeirinha-RS 2012
- Eriksson , L. Super Clean Steel Improves Fatigue Properties of Valve Springs Oak Brook, IL Spring Manufacture Institute, USA March 1995 34 47 55
- Lund , T. B. , Ölund , L. J. P. Improving Production, Control and Properties of Bearing Steels Intended for Demanding Applications Advances in the Production and Use of Steel with Improved Internal Cleanliness Mahaney J. K. , Jr. American Society for Testing and Materials 1999
- Blair , M. , Monroe , R. W. , and Griffin , J. A. A Review and Update of Advancements in Clean Cast Steel Technology Advances In The Production and Use of Steel with Improved Internal Cleanliness Mahaney J. K. , Jr. American Society for Testing and Materials West Conshohocken, PA 1999
- Wilson , A. D. Clean Steel Technology - Fundamental to the Development of High Performance Steels Advances In The Production and Use of Steel with Improved Internal Cleanliness Mahaney J. K. , Jr. American Society for Testing and Materials West Conshohocken, PA 1999
- Colpaert , H. Metalografia dos produtos siderúrgicos comuns Blucher publishing house 4 2008
- Senthilkumar , D. , Rajendran , I. , and Pellizzari , M. Effect of cryogenic treatment on the hardness and tensile behaviour of AISI 4140 steel International Journal Microstructure and Materials Properties 2011 6 5 366 377
- Dowling , N. E. Mechanical Behavior of Materials Engineering Methods for Deformation, Fracture and Fatigue Pearson Prentice Hall 3 2007
- Chang , W. Applying similarity methods to fracture mechanics-measurement of fracture toughness K IC , K Q values by small-scale single specimen Eng. Fract. Mech. 1988 31 807 816
- Chang , W. An improvement of applying similarity methods to fracture mechanics-measurement of fracture toughness K IC , K Q values by smallscale single specimen Eng. Fract. Mech. 1990 36 313 320
- Vitek , V. , Chell , G. G. An assessment of some post-yield fracture criteria Mater. Sci. Eng. 1977 27 209 215
- Šuštaršič , B. , Leskovšek , V. , Juriša , G. Fracture-toughness K IC of HSS AISI M-2 type Mater. Technol. 2003 37 6 369 376
- Ule , B. , Leskovšek , V. , Tuma , B. Estimation of plain strain fracture toughness of AISI M2 steel from precracked round-bar specimens Eng. Fract. Mech. 2000 65 559 572
- Li , D. M. , Bakker , A. Fracture toughness evaluation using circumferentially-cracked cylindrical bar specimens Eng. Fract. Mech. 1997 57 1 1 11
- Ewalds , H. L. , Wanhill , R. J. H. Fracture mechanics Edward Arnold Ltd. London, U. K. 1985
- Janssen , M. , Zuidema , J. , Wanhill , R. J. H. Fracture Mechanics 2nd Delft University Press Delft, Netherlands 2002