Microstructure and Wear Behavior of Austempered and as-cast Ausferritic Gray Cast Irons

2011-26-0051

01/19/2011

Event
SIAT 2011
Authors Abstract
Content
The mechanical and wear behaviour of an alloyed gray cast iron with ausferrite microstructure directly obtained on solidification has been compared with austempered alloyed gray iron. As-cast ausferritic gray iron shows finer ausferrite and graphite flake morphology compared to austempered alloy. The volume of retained austenite is about 30% higher in as-cast ausferritic iron due to higher amount of alloying additions. The mechanical and wear properties of as-cast ausferritic iron are almost similar to austempered alloy.
Meta TagsDetails
DOI
https://doi.org/10.4271/2011-26-0051
Pages
4
Citation
Vadiraj, A., and Kamaraj, M., "Microstructure and Wear Behavior of Austempered and as-cast Ausferritic Gray Cast Irons," SAE Technical Paper 2011-26-0051, 2011, https://doi.org/10.4271/2011-26-0051.
Additional Details
Publisher
Published
Jan 19, 2011
Product Code
2011-26-0051
Content Type
Technical Paper
Language
English