This content is not included in your SAE MOBILUS subscription, or you are not logged in.

Mechanical Properties of Polymer Composites Used in Oxidizing Environments: A Review

Journal Article
2010-01-0026
ISSN: 1946-3979, e-ISSN: 1946-3987
Published April 12, 2010 by SAE International in United States
Mechanical Properties of Polymer Composites Used in Oxidizing Environments: A Review
Sector:
Citation: Jones, D., Pulla, S., and Lu, Y., "Mechanical Properties of Polymer Composites Used in Oxidizing Environments: A Review," SAE Int. J. Mater. Manuf. 3(1):63-70, 2010, https://doi.org/10.4271/2010-01-0026.
Language: English

References

  1. Patekar K. A. “Long term Degradation of Resin for High Temperature Composites,” Final Contractor Report NASA CR-2000-209918 2000
  2. Bowles K. J. Papadopoulos D. J. Inghram L. L. McCorkle L. S. Klan O. V. “Longtime durability of PMR-15 matrix polymer at 204, 260, 288 and 316 °C,” NASA/TM-2001-210602 2001
  3. Schoeppner G. A. Tandon G. P. Pochiraju K. V. “Predicting Thermo-Oxidative Degradation and Performance of High Temperature Polymer Matrix Composites,” Multiscale Modeling and Simulation of Composite Materials and Structures Springer 2007 359 462
  4. Tandon G. P. Pochiraju K. V. Schoeppner G. A. “Modeling of oxidative development in PMR-15 resin,” Polymer Degradation and Stability 91 8 1861 1869 2006
  5. Pochiraju K. V. Tandon G. P. “Modeling thermo-oxidation layer growth in high temperature resins,” Journal of Engineering Materials and Technology 128 1 107 116 2006
  6. Regnier N. Berriot J. Lafontaine E. Mortaigne B. “Spectromechanical analysis of the structure and oxidation of PMR thermoset thermally-stable resins,” Polymer Degradation and Stability 73 3 485 490 2001
  7. Meador M. A. B. Lowell C. E. Cavano P. J. Herrera-Fierro P. “On the oxidative degradation of nadic endcapped polyimides: I. Effect of thermocycling on weight loss and crack formation,” High Performance Polymers 8 3 363 379 1996
  8. Meador M. A. B. Johnston J. C. Cavano P. J. Frimer A. A. “On the oxidative degradation of nadic endcapped polyimides: 2. Evidence for reactions occurring at high temperature,” Macromolecules 30 11 3215 3223 1997
  9. Meador M. A. B. Johnston J. C. Frimer A. A. Gilinsky-Sharon P. “On the oxidative degradation of nadic endcapped polyimides: 3. Synthesis and characterization of model compounds for end-cap degradation products,” Macromolecules 32 17 5532 5538 1999
  10. Odegard G. Kumosa M. “Elastic-plastic and failure properties of a unidirectional carbon/PMR-15 composite at room and elevated temperatures,” Composite Science and Technology 60 16 2979 2988 2000
  11. Broeckert J. L. “Effects of Prior Aging at Elevated Temperature in Air and in Argon Environments on Creep Response of PMR-15 Neat Resin at 288°C,” Master's Thesis WPAFB OH 2007
  12. Falcone C. M. “Some Aspects of the Mechanical Response of PMR-15 Neat Resin at 288 °C; Experiment and Modeling,” Master's Thesis WPAFB OH 2006
  13. Robinson G. W. “High temperature Chemical Degradation of PMR-15 Polymer Resins,” Master's Thesis WPAFB OH 2005
  14. Westberry C. M. “Rate Dependence and Short-Term Creep Behavior of PMR-15 Neat Resin at 23 and 288°C,” Master's Thesis WPAFB OH 2005
  15. Back C. A. “Effects of Prior Aging on the Creep Response of Carbon Fiber Reinforced PMR-15 Neat Resin at 288ˆC in an Air Environment,” Master's Thesis WPAFB OH 2007
  16. Xie W. Pan W.-P. Chuang K. C. “Thermal characterization of PMR polyimides,” Thermochimica Acta 367-368 143 153 2001
  17. Patekar K. A. “Long term Degradation of Resin for High Temperature Composites,” Final Contractor Report NASA CR-2000-209918 2000
  18. Bowles K. J. Papadopoulos D. J. Inghram L. L. McCorkle L. S. Klan O. V. “Longtime durability of PMR-15 matrix polymer at 204, 260, 288 and 316 °C,” NASA/TM-2001-210602 2001
  19. Tsuji L. C. McManus H. L. Bowles K. J. “Mechanical properties of degraded PMR-15 resin,” NASA/TM-1998-208487 1998
  20. Lu, Y.C. Tandon G. P. Jones, D.C. Schoeppner G. A. “Elastic and viscoelastic characterization of thermally-oxidized polymer resin using nanoindentation” Journal of Mechanics of Time-Dependent Materials 13 245 260 2009
  21. Chen, R Lu, Y.C. Yang, F Tandon, G.P. Schoeppner, G.A. “Impression Creep of PMR-15 Resin at Elevated Temperatures” Polymer Engineering and Science 50 1 209 213 2010
  22. Lu, Y.C. Tandon G. P. Putthanarat, S Schoeppner G. A. “Nanoindentation strain rate sensitivity of PMR-15 Polyimide” Journal of Materials Science 44 2119 2127 2009
  23. Lu, Y.C. Jones D. C. Tandon G. P. Putthanarat, S Schoeppner G. A. “High Temperature Nanoindentation of PMR-15 Polyimide” Experimental Mechanics 2010 10.1007/s11340-009-9254-5
  24. Johnson L. L. Eby R. K. Meador M. A. B. “Investigation of oxidation profile in PMR-15 polyimide using atomic force microscope (AFM),” Polymer 44 1 187 197 2003
  25. Oliver W. C. Hutchings R. Pethica J. B. “Measurement of Hardness at Indentation Depths as Low as 20 Nanometres,” Microindentation Techniques in Materials Science and Engineering ASTM 1985
  26. Pharr G. M. Harding D. S. Oliver W. C. “Measurement of fracture toughness in thin films and small volumes using nanoindentation methods,” NATO Advanced Study Institute on Mechanical Properties of Materials Having Ultra-Fine Microstructure Porto Novo, Portugal 1992

Cited By