This content is not included in
your SAE MOBILUS subscription, or you are not logged in.
Testing Study of Temperature Field of Bias Tire made in China
Technical Paper
2003-01-0313
ISSN: 0148-7191, e-ISSN: 2688-3627
Annotation ability available
Sector:
Language:
English
Abstract
9.00-20 P.R12 (nylon cords and longitudinal patterns) bias tire made in China is tested by the designed infrared thermometer system and thermocouple. External surface temperatures of the tire are measured by the infrared thermometer, internal temperature of the tire is obtained by calculation with measured data, and body temperatures of the tire are measured by the thermocouples inserted into holes, which have been drilled into some parts of tire. The influence of operating conditions such as time and speed on tire temperature field distributions is also analyzed. The experimental results lay foundation for reasonably selecting types of tire and determining the limited operations of a tire, and supplying numerical analysis with essential boundary conditions.
Recommended Content
Authors
- Li Jie - National Automobile Dynamic Simulation Laboratory, Jilin University, P. R. China
- Zhao Qi - National Automobile Dynamic Simulation Laboratory, Jilin University, P. R. China
- Wang Qingnian - National Automobile Dynamic Simulation Laboratory, Jilin University, P. R. China
- Zhao Ziliang - National Automobile Dynamic Simulation Laboratory, Jilin University, P. R. China
Topic
Citation
Jie, L., Qi, Z., Qingnian, W., and Ziliang, Z., "Testing Study of Temperature Field of Bias Tire made in China," SAE Technical Paper 2003-01-0313, 2003, https://doi.org/10.4271/2003-01-0313.Also In
References
- Clark S.K. “Temperature Rise Times in Pneumatic tires” Tire Science and Technology 4 171 189 1976
- Ziliang Zhao “Temperature Field Study of a High Rolling Automobile Tire” Master's paper Jilin University of Techenology 1998
- Ziliang Zhao “Predicted Model Study of a High Rolling Automobile Tire” Ph.D. Dissertation ilin University 2001