AMS5663N Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 52.5Ni - 19Cr - 3.0Mo - 5.1Cb (Nb) - 0.90Ti - 0.50Al - 18Fe Consumable Electrode or Vacuum Induction Melted 1775 °F (968 °C) Solution and Precipitation Heat Treated

Revised

06/20/2016

Features
Issuing Committee
Scope
Content
This specification covers a corrosion and heat-resistant nickel alloy in the form of bars, forgings, flash welded rings up to 10 inches (254 mm) in least cross-sectional dimension, having a maximum cross-sectional area of 78 in2 (503 cm2), and stock of any size for forging or flash welded rings (see 8.5).
Rationale
Content
AMS5663N revises Composition (Table 1), Condition (3.3), Properties (3.5, Tables 2 and 3), added properties for product up to 10 inches (254 mm) in diameter or least distance between parallel sides, adds conformance to AS6279 (3.8), revises Reports (4.4), and is a Five Year Review and update of this specification.
Meta TagsDetails
DOI
https://doi.org/10.4271/AMS5663N
Pages
11
Citation
SAE International Material Specification, Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 52.5Ni - 19Cr - 3.0Mo - 5.1Cb (Nb) - 0.90Ti - 0.50Al - 18Fe Consumable Electrode or Vacuum Induction Melted 1775 °F (968 °C) Solution and Precipitation Heat Treated, SAE Standard AMS5663N, Revised June 2016, Reaffirmed June 2009, Issued September 1965, https://doi.org/10.4271/AMS5663N.
Additional Details
Publisher
Published
Jun 20, 2016
Product Code
AMS5663N
Content Type
Material Specification
Status
Revised
Language
English

Revisions

Historical