AMS2759/1D Heat Treatment of Carbon and Low-Alloy Steel Parts Minimum Tensile Strength Below 220 ksi (1517 MPa)

Revised

06/13/2007

Features
Issuing Committee
Scope
Content
This specification, in conjunction with the general requirements for steel heat treatment covered in AMS 2759, establishes the requirements for heat treatment of carbon and low-alloy steel parts to minimum ultimate tensile strengths below 220 ksi (1517 MPa). Parts are defined in AMS 2759.
Rationale
Content
AMS 2759/1D results from a Five Year Review and update of this specification.
Meta TagsDetails
DOI
https://doi.org/10.4271/AMS2759/1D
Pages
12
Citation
SAE International Material Specification, Heat Treatment of Carbon and Low-Alloy Steel Parts Minimum Tensile Strength Below 220 ksi (1517 MPa), SAE Standard AMS2759/1D, Revised June 2007, Issued October 1984, https://doi.org/10.4271/AMS2759/1D.
Additional Details
Publisher
Published
Jun 13, 2007
Product Code
AMS2759/1D
Content Type
Material Specification
Status
Revised
Language
English