Scope
Content
This document establishes the requirements for the sequencing of processes relating to parts fabricated from 300M or 4340 modified steel heat treated to, or to be heat treated to, 270,000 psi (1860 MPa) minimum ultimate tensile strength (UTS) and higher.
Rationale
Content
ARP1631A has been reaffirmed to comply with the SAE five-year review policy.
Meta TagsDetails
DOI
https://doi.org/10.4271/ARP1631A
Pages
12
Citation
SAE International Recommended Practice, Manufacturing Sequence for Fabrication of High-Strength Steel Parts 300M or 4340 Modified Low-Alloy Steels 270,000 psi (1860 MPa) Tensile Strength and Higher, SAE Standard ARP1631A, Reaffirmed September 2018, Revised November 2007, Issued October 1984, https://doi.org/10.4271/ARP1631A.
Additional Details
Publisher
Published
Sep 27, 2018
Product Code
ARP1631A
Content Type
Recommended Practice
Status
Reaffirmed
Language
English

Revisions