Determining Decarburization and Carburization in Finished Parts of Carbon and Low-Alloy Steels
- Aerospace Standard
- ARP1341B
- Reaffirmed
Scope
Recommended Content
Aerospace Material Specification | Heat Treatment of Carbon and Low-Alloy Steel Parts Minimum Tensile Strength Below 220 ksi (1517 MPa) |
Aerospace Material Specification | Heat Treatment of Low-Alloy Steel Parts Minimum Tensile Strength 220 ksi (1517 MPa) and Higher |
Aerospace Material Specification | Steel, Corrosion-Resistant, Investment Castings 16Cr - 1.9Ni - 0.08N As Cast |
Data Sets - Support Documents
Title | Description | Download |
---|---|---|
Unnamed Dataset 1 |
Issuing Committee
AMS B Finishes Processes and Fluids Committee
The committee of Finishes, Processes, and Fluids, AMS Committee B, shall prepare, coordinate, and revise documents related to processing technology, such as plating, brazing, coatings and compounds, through the participation of process suppliers, users, and interested government agencies. Committee activities shall provide a forum for the cooperative interchange of ideas and experience of the participants, resulting in the publication of specifications that embody sound, established aerospace industry practices and requirements to serve the suppliers and customers of aerospace processes.
Reference
Number | Title |
---|---|
ASTME3 | This document is not part of the subscrption. |
ASTME384 | This document is not part of the subscrption. |
ASTME407 | This document is not part of the subscrption. |