AMS5630K Steel, Corrosion-Resistant, Bars, Wire, and Forgings 17Cr - 0.52Mo (0.95 - 1.20C) (440C)
Revised
01/06/2012
- Features
- Issuing Committee
- Content
- This specification covers a corrosion-resistant steel in the form of bars, wire, forgings, and forging stock.
- Content
- AMS5630K adds a requirement that bar not be cut from plate (3.2.1/4.4.2), adds requirements for micro-cleanliness (3.3.2), grain size (3.3.3), conformance to AMS2303 (3.4.1), changes decarburization from a periodic to an acceptance test (4.2.1), revises Reports (4.4), and results from a Five Year Review and update of this specification.