Content
This specification, in conjunction with the general requirements for steel heat treatment covered in AMS2759, establishes the requirements for heat treatment of low-alloy steel parts to minimum ultimate tensile strengths of 220 ksi (1517 MPa) and higher. Parts are defined in AMS2759.
Rationale
Content
AMS2759/2E is an update to remove 300M from 3.4.7 and Table 2 Note 2. AMS 2759/2D resulted from a Five Year Review and update to include in Table 2 Note 5 clarification that the snap temper is employed before refrigeration. AMS 2759/2D also included use of marquenching.
Meta TagsDetails
DOI
https://doi.org/10.4271/AMS2759/2E
Pages
12
Citation
SAE International Material Specification, Heat Treatment of Low-Alloy Steel Parts Minimum Tensile Strength 220 ksi (1517 MPa) and Higher, SAE Standard AMS2759/2E, Revised July 2009, Issued October 1984, https://doi.org/10.4271/AMS2759/2E.
Additional Details
Publisher
Published
Jul 20, 2009
Product Code
AMS2759/2E
Content Type
Material Specification
Status
Revised
Language
English