Abstract
Over the past 20 years, polyvinyl chloride (PVC) has almost replaced metal in stationary glass reveal moldings with dramatic part cost savings on cars and trucks world-wide. The process of assembly is generally simple and convenient but to replace a reveal molding can be difficult. Many times, in order to replace the molding, it may also be necessary to replace or reseal the glass. In short, PVC reveal moldings, relatively inexpensive parts, are very expensive to service.
Outside of general assembly and processing issues, there are 5 variables that may cause a failure in the performance of a stationary glass reveal molding. They are as follows: material degradation, crystallization, plasticizer loss, material properties, and molded-in stress. Because of modern standard PVC formulations and the material requirements of most automotive companies, material degradation, crystallization and plasticizer loss do not commonly cause failure. Material properties and molded-in stress do.
The automotive industry has developed many extreme-temperature component tests to model PVC reveal molding failures seen on full vehicle tests without a thorough understanding of the mechanism of failure. These test methods, although effective, are expensive and require engineering time.
By understanding the PVC failure mechanism and standardizing a test method for evaluating these and similar parts, engineering time efficiency will be improved, OEM PVC molding suppliers will be less confused by many different required testing procedures, and testing costs will be significantly reduced if not eliminated. This paper reviews the 5 variables above and suggests a simple standardized procedure developed from tested parts which eliminates the future need for an elaborate validation test.
Authors
Citation
Ferris, T., Finken, M., Dziadzio, B., and Bishop, T., "Accelerated Glass Reveal Molding Test," SAE Technical Paper 980718, 1998, https://doi.org/10.4271/980718.Also In
References
- Handbook of Materials and Technology Rubin Irwin I. John Wiley and Sons, Inc. 1990 1567
- Kirk-Othmer Encyclopedia of Chemical Technology John Wiley & Sons, Inc. USA 1978 896 898 23
- Encyclopedia of PVC Nass Leonard I. Heiberger Charles A. Marcel Dekker, Inc. 270 Madison Ave., NY, NY 10016 1992 160 3
- SAE J1960 June 1989 Accelerated Exposure of Automotive Exterior Materials Using A Controlled Irradiance Water-Cooled Xenon Arc Apparatus
- Polmer Science and Technology Fried Joel R. Prentice Hall PTR Edgewood Cliffs, NJ, 07623 1995 19
- Handbook of Polyvinyl Chloride Formulating Wickson Edward J. 1993 John Wiley & Sons, Inc. 605 Third Avenue, New York, NY 10158-0012 18
- “Crystallinity In Poly(Vinyl Chloride)” Gilbert Marianne J. Macromol Sci Rev Macromol Chem Phys c34 1 Feb 1994 77 135
- Polmer Science and Technology Fried Joel R. Prentice Hall PTR Edgewood Cliffs, NJ, 07623 1995 65
- Polmer Science and Technology Fried Joel R. Prentice Hall PTR Edgewood Cliffs, NJ, 07623 1995 144
- PVC Plastics: Properties, Processing and Applications Titow W. V. Elsevier Science Publishers Co., Inc. 1990 195
- Choi S. Y. 1993 SAE Technical Paper No. 931955
- PVC Plastics: Properties, Processing and Applications Titow W. V. Elsevier Science Publishers Co., Inc. 1990 242
- Plastics Additives Handbook Gachter R. Muller H. Andreas H. Scientific and Technical Books Macmillan Publishing Co. 866 Third Ave. New York, N.Y. 10022 1984 264 265
- Standard Test Methods for Volatile Loss from Plastics Using Activated Carbon Methods
- Standard Practice for Testing Plasticizer Compatibility in Poly(Vinyl Chloride) (PVC) Compounds Under Humid Conditions
- Standard Test Method for Analysis of Components in Poly(Vinyl Chloride) (PVC) Compounds Using an Infrared Spectrophotometric Technique
- Standard Test Method for Analysis of Components in Poly(Vinyl Chloride) (PVC) Compounds Using an Infrared Spectrophotometric Technique Choi S. Y.
- Handbook of Plastics Test Methods Ives Mead Riley Butterworth Group 1971 298 299
- Beaumont J. P. 1989 SAE Technical Paper No. 890626
- Bernhardt E. C. Bernhardt M. R. 1989 SAE Technical Paper No. 890627
- Bernhardt M. G. 1986 SAE Technical Paper No. 860284
- Winkler M. 1992 SAE Technical Paper No. 920504
- Standard Practice for Estimating the Quality of Molded Poly(Vinyl Chloride) (PVC) Plastic Pipe Fittings by the Heat Reversion Technique
- Willis Mike Vice-President Of Quality Joint Study Between General Motors And Plastic Trim, Inc. May 3 1996
- Polmer Science and Technology Fried Joel R. Prentice Hall PTR Edgewood Cliffs, NJ, 07623 1995 252 253
- PVC Plastics: Properties, Processing and Applications Titow W. V. Elsevier Science Publishers Co., Inc. 1990 203
- Polmer Science and Technology Fried Joel R. Prentice Hall PTR Edgewood Cliffs, NJ, 07623 1995 155